”Shrink-free grout” with high interim and final strength must be used for normal grouting heights of 50 mm.
General reference values for ***a.m. grouts***:
Pot life after preparation
one hour
(at + 20 °C)
Minimum application temperature (also components)
+ 5° C
Dry mortar, weight
1.900 kg/m3
Compressive strength after one day
50 N/mm2
Compressive strength after 28 days
90 N/mm2
Flexural and tensile strength after one day
6 N/mm2
Flexural and tensile strength after
28 days
9 N/mm2

díky předem!

Proposed translations

39 mins

spárovací hmoty (značky) AM

Našel jsem na internetu tuto firmu. Podobnost však může být čistě náhodná.
Something went wrong...
1 day 8 hrs

(Samo) (nivelační) stěrka

Dle níže uvedených parametrů by se mohlo jednat o stěrku.
Something went wrong...
Term search
  • All of ProZ.com
  • Term search
  • Jobs
  • Forums
  • Multiple search